DIN1.2379 hot rolled tool steel
  • FOB Price
    US $ 1.00 / Ton(s)
  • Min. Order
    10 Ton(s)
  • Payment Terms
    -- --
  • Port
    wuhan, shenzhen, shanghai
  • Delivery Time
    0 days after payment
  • Steel Grade:
    D2/Cr12Mo1V1/DIN1.237...
  • Standard:
    AISI, ASTM, DIN, GB, ...
  • Dimensions:
    Square/Round Bar: 12m...
  • Place of Origin:
    Hubei China (Mainland...
  • Brand Name:
    unite
  • Model Number:
    Flat:10-155mmx50-610m...
  • Technique:
    Hot Rolled
  • Application:
    Tool Steel Bar
  • Alloy Or Not:
    Is Alloy
  • Special Use:
    Mold Steel
  • Type:
    Alloy Steel Bar
  • Ultrasonic Test:
    According with SEP 19...
Product Description

D2/DIN 1.2379

 

Description:

12% chrome steel, very high resistance against abrasive and adhesive wear due to a high volume of hard carbides in the steel matrix, good toughness, very good dimensional stability, high compressive strength, very good base material for PVD/CVD coating as well as nitriding due to its secondary hardening properties. Similar to AISI D2.


Applications: Excellent toughness and suitable for bath nitriding. Cold extrusion tools, trimming, cutting and stamping tools for sheet thickness upto 6mm, precision cutting tools for sheet thickness up to 12.2 mm. Blaniking and punching tools, wood working tools, shear blades for cutting light gauge material, thread rolling dies , drawing, deep drawing, Pressure pads and highly wear-resistant plastic moulds.

Steel Grade:

GB  Cr12Mo1V1

C

Si

Mn

P

S

Cr

Mo

V

1.40-1.60

<= 0,60

<=0,60

<= 0,030

<= 0,030

11,00 - 13,00

0.70 -1.20

0.50 -1.10

DIN-1.2379,%

C

Si

Mn

P

S

Cr

Mo

V

1,50 - 1,60

0,20 - 0,60

0,15 - 0,45

<= 0,030

<= 0,030

11,00 - 12,00

0,60 - 0,80

0,90 - 1,10

Similar grade:AISI-D2, SKD11,DC11,K100. DIN 1.2379

Delivery Condition:

 

GB/T1299-2000

DIN

AISI

  Annealed (HB)

<=255

<=250

255~217

Size available:

Square/Round Bar: 12~ 75mm

Flat:10~155x 50~ 610mm

 

Forging:
Heat slowly and uniformly to 700°C then more rapidly to 900/1040°C.  After forging cool slowly.

Annealing:
Anneal at 850°C and slow furnace cool. Hardness after annealing will be approx. 225 brinell.
Hardening:
Pre heat slowly to 750/780°C and thoroughly soak. Continue heating to the final hardening temperature of 1000/1030°C and allow the component to be heated through. Quench in oil or cool in air.
Tempering:
Heat uniformly and thoroughly at the selected tempering temperature and hold for at least one hour per inch of total thickness. Double tempering should be carried out with intermediate cooling to room temperature.
Stress Relieving:
If machining operations have been heavy or if the tool has an unbalanced section, remove stresses before hardening by heating up to 700°C, equalise, then cool slowly.
Hard Chromium Plating:
After hard chromium plating tempering of D2 tool steel is recommended at 180°C for 4 hours to avoid hydrogen embrittlement.  Tempering is to be performed immediately after chromium plating.

Welding:
Due to the high risk of crack formation welding of D2 tool steel should be avoided, if possible. When, howe ver welding is essential, the following serves as a guide:
A.   Welding of soft annealed D2 tool steel.
·       Preheat to 300 - 500°C
·       Weld at 300-500°C
·       Immediately stress relieve
Electrode: Cr-Mo alloy electrode for welding structural steel.
B.    Welding in connection with hardening of soft annealed D2 tool steel.
·       Heat to austenitizing temperature.
·       Cool to approx. 500°C
·       Weld at approx. 500°C
·       Cool to approx. 100°C in the same way as at normal hardening, then temper to desired hardness. Double tempering will
     reduce the risk of crack formation.
Electrode: Hard facing electrode.
C.    Repair welding of D2 tool steel in hardened and tempered condition.
·       Preheat to the tempering temperature (min. 200°C) previously used.
·       Weld at tempering temperature
·     Heat immediately to tempering temperature, but max. 300°C. Soaking time 2 hours.
Electrode: Hard facing electrode.