Product Code: 112353123

Address:

,China

Main Products:

tool steel,alloy steel,high tensile,bearing steel,case hardening

Contact Info.
DIN1.2080 hot forged tool steel
  • FOB Price
    US $ 1.00 / Ton(s)
  • Min. Order
    10 Ton(s)
  • Payment Terms
    -- --
  • Port
    wuhan, shenzhen, shanghai
  • Delivery Time
    0 days after payment
  • Steel Grade:
    D3/Cr12/DIN1.2080/SKD...
  • Standard:
    AISI, ASTM, DIN, GB, ...
  • Dimensions:
    Square/Round Bar: 80m...
  • Place of Origin:
    Hubei China (Mainland...
  • Brand Name:
    unite
  • Model Number:
    Flat:30-155mmx50-800m...
  • Technique:
    Forged
  • Application:
    Die Steel Bar
  • Alloy Or Not:
    Is Alloy
  • Special Use:
    Mold Steel
  • Type:
    Alloy Steel Bar
  • Ultrasonic Test:
    According with SEP 19...
Product Description

D3/DIN 1.2080


Description:

D3 is an oil hardening, high Carbon/ Chromium type tool steel with very high wear resistance. It hardens with a very slight change in size. The alloy possesses very high compressive strength and is deep hardening.

 

Applications: High performance cutting tools for sheet upto 4mm Thickness, trimming dies, blanking

dies for paper and plastic,shear blades for cutting light gauge material, thread rolling dies , drawing, deep drawing, Pressure pads and highly wear-resistant plastic moulds.

Principal Design Features

Machinability
The machinability rating of D3 is roughly 25% that of free machining carbon steel 1018.. Due to its abrasion resistant nature, machining in the hardened condition should be limited to finish grinding.

 

Heat Treatment
Maximum properties are achieved through the process of hardening and tempering. See the processes below. For maximum accuracy, parts should be stress relieved after roughing operations. Stress relieve at 1200F for one hour and cool slowly.
Annealing
Annealing should be performed in a controlled atmosphere furnace. Heat thoroughly to 1600 F and cool slowly, at a rate of not more than 20 F per hour, until furnace is black. Material may then be removed and air cooled.
Tempering
After cooling to room temperature, parts should be tempered immediately. Place parts in the tempering furnace and raise slowly to desired tempering temperature. Temper for 1 hour per inch of thickness.
Hardening
Do not overheat this material, it is very sensitive to overheating and will not achieve maximum hardness if heated improperly. Harden by placing the work directly into a furnace preheated to 1750F and soak for 20-25 minutes, plus 5 minutes per inch of th.

 

Steel Grade:
GB   Cr12

C

Si

Mn

P

S

Cr

2.0 - 2,30

<= 0,40

<=0,40

<= 0,030

<=0,030

11,50 - 13,00

DIN-1.2080  

C

Si

Mn

P

S

Cr

1,90 - 2,20

0,10 - 0,40

0,15 - 0,45

<= 0,030

<= 0,030

11,00 - 12,00

Similar grade:AISI-D3,JIS-SKD1, DIN 1.2080

Delivery Condition:

 

GB/T1299-2000

DIN

AISI

Annealed (HB)

269~217

<=250

255~217

Harden(HRC)

58~60

57~63

54~61

Size available:

Square/Round Bar: 12~ 80mm

Flat:10~155x 50~ 610mm