Product Code: 112352943

Address:

,China

Main Products:

tool steel,alloy steel,high tensile,bearing steel,case hardening

Contact Info.
S136 Hot Forged Plastic Mould Steel Bar
  • FOB Price
    US $ 2.00 - 3.00 / Ton(s)
  • Min. Order
    10 Ton(s)
  • Payment Terms
    -- --
  • Port
    wuhan, shanghai, shenzhen
  • Delivery Time
    0 days after payment
  • Steel Grade:
    S136/4Cr13/DIN1.2083/...
  • Standard:
    AISI, ASTM, BS, DIN, ...
  • Dimensions:
    Square/Round Bar: 12~...
  • Place of Origin:
    Hubei China (Mainland...
  • Brand Name:
    unite
  • Model Number:
    Flat: thickness,20~ 3...
  • Technique:
    Forged
  • Application:
    Die Steel Bar
  • Alloy Or Not:
    Is Alloy
  • Special Use:
    Mold Steel
  • Type:
    Alloy Steel Bar
  • Ultrasonic test:
    According to SEP 1921...
Product Description

S136/ DIN 1.2083

 

Description: 1.2083 is a chromium alloyed stainless plastic mould steel, which is characterised by good polishability, good hardenability giving high hardness, with fair corrosion resistance.

Application: applied in all plastic mould, especially used in transparent plastic mould for CD disk, optical equipment mould and those with low acid environment.

Steel Grade:

GB  4Cr13, %

C

Si

Mn

P

S

Cr

0,36 - 0,45

<=0,60

<= 0,80

<= 0,035

<= 0,030

12,00 -14,00

DIN- 1.2083 %

C

Si

Mn

P

S

Cr

0,36 - 0,42

<= 1,00

<= 1,00

<=0,030

<= 0,030

12,50 - 14,50

Similar grade: AISI-420,S136/136H, M310,FT64.

Delivery Condition:

 

GB/T1299-2000

DIN

Annealed (HB)

320~285

<=225

Harden(HRC)

30~35

 

Size available:

Square/Round Bar: 12~ 450mm

Flat: thickness,20~ 350mm , width, 500mm - 800mm ,

Length: Contracted.

 

Forging:
Heat slowly and uniformly to 1000°C. After forging cool slowly.  

Annealing:
Heat slowly to 780°C. Slowly cool in furnace.
Hardening:
Pre heat to 600-700°C until heated through. (Austenitizing temperature 1025°C.) Continue heating to the final hardening temperature of 980-1050°C and allow the component to be heated through.  Protect against decarburisation by using neutral salt bath, controlled atmosphere furnace or vacuum. Air cool or quench in oil.
Tempering:
Heat uniformly and thoroughly at the selected tempering temperatures and hold at heat for one hour per inch of total thickness. Double tempering is recommended.
Nitriding:
Nitriding of 1.2083 gives it a hard surface which is very resistant to wear and corrosion. Howe ver , the nitrided surface reduces the corrosion resistance. Surface hardness after nitriding at 525°C in ammonia gas will be approximately 1000HV.

Welding:
Due to the high risk of crack formation welding of 1.2083 stainless steel should be avoided, if possible. When, howe ver welding is essential, the following serves as a guide:
A.  Welding of soft annealed 1.2083 stainless steel.
·       Preheat to 300 - 500°C
·       Weld at 300-500°C
·       Immediately stress relieve
B.  Repair welding of 1.2083 stainless steel in hardened and tempered condition.
·       Preheat to the tempering temperature (min. 200°C) previously used.
·       Start welding  at tempering temperature
·       Re heat immediately to tempering temperature, but max. 300°C. Soaking time 3 hours.
·       Cool in air to approximately 80°C.
·       Re heat immediately to tempering temperature, but max. 300°C. Soaking time 3 hours.